Taggers right, the only one that was 24 hrs was the straight val oil. I thought 24 would be way too long for the thin stuff.
Maybe Capesam was onto something with the temperature too as it is cold in my garage where I did all the sealing (40 or so at night), and the turp stuff smelled so bad I did not bring them into the warmer part of the basement near the furnace for a couple of days. I wish I'd done just a piece of unsealed wood too, to have it to compare too the others to see how much it absorbed and too see the difference sealing it made.
I've still got the stuff, I could do another test. I think i've got some 5/4 pine left over from a xmas project... If I do another test on a softer wood do you think that would be a more valid test. how long should i let em soak...what do you want to see ?
|