Quote:
Originally Posted by Woodbuster
What is the pot life on the CPES?
Are there different hardeners for different times like West Systems?
|
They make 2 formulas, warm and cold. Warm is for 86deg down to 50deg with a pot life from 4hrs at 86deg to 16hrs at 50deg.The cold formula is for below 50deg with a pot lfe of 8 hrs.
Priming is optional.