Quote:
Originally Posted by ProfessorM View Post
Here are a few conrad lips I cooked at 1000 degrees for 1 hour and cooled slowly. They will be put on skin plugs I am doing. I like the no shine look for nite time.
looks like your trying to match the color of the eel skins inside out.

we use to have some stuff to parkerize[spelling?] metal..it wa a blue liquid that you heated to 150* degrees and you'd just let the metal soak in it for an hour..it would come out dark charcoal grey and never come off....the army would use it kill the shine on their equipment.