Update on SYS 3
Took a bunch of the good advice here and employed it with much better results:
1. Nitrile gloves worn for assembly instead of bare hands.
2. Precision mixing and bigger batches.
3. Kept plugs in warm room after finishing, but away from furnace.
4. Plastic stirrer instead of popsicle stick.
Stuff is hard as a rock after 72 hours with no obvious marbling. Will wait until they go in the water before I declare victory as much of the marbling was occurring after I dunked the plugs.
|