I used a 2 part finish that uses an acid catalyst. I had no time to use 2 part urethane like I wanted to since they could not wait the 21 days it would take for full cure and it would show scratches all over, so it was cheaper and quicker this way. They are happy and it looks great. I used commercial conversion varnish in satin for the rest of the furnishings.