Yes i hear u. I e texed my first batch. Came out great. Too time consuming for 100. Heat treated and use 60/40 spar. Sucked in 7 gr. Ok I said good penetration. dry 1 week. Sands good. But the amount internally was not dry and bleed thru and lifted the paint and epoxy. I stripped them and they stunk of spar mixture. They are drying for a few weeks. Stink gone . I will prime with gold label zinseer and hope for the best.