Fly head cement
Not about plugs but tail hooks. I have been finishing my heads with Waspi Gloss Coat Head Cement,
On the advice of someone here I bought a kid of UV Glue. I have been applying the UV Glue over the Gloss head cement after the Gloss is dry. The UV Glue finish is great except for one problem. After I use the UV light on it and it dries, it tacky.
Has anyone else had this problem?
|
No boat, back in the suds.
|
|
|
01-29-2023, 09:25 AM
|
#2
|
Registered User
Join Date: Dec 2002
Location: North Branford,Ct.
Posts: 7,588
|
Never used UV. Heard it used on lure finish. I use for teasers and flags Flexcoat hi build. Coat it and spin it. Takes about 6 hrs. A quicker method is 15 min rod adhesive epoxy. Sets up within 30min. Let dry. I thin a little w/isopropyl alcohol to make it flow around the thread wrap.
BTW the hook teasers look real nice.
Posted from my iPhone/Mobile device
|
|
|
|
01-29-2023, 09:49 AM
|
#3
|
Very Grumpy bay man
Join Date: Nov 2003
Location: Rhode Island
Posts: 10,666
|
Quote:
Originally Posted by pbadad
Never used UV. Heard it used on lure finish. I use for teasers and flags Flexcoat hi build. Coat it and spin it. Takes about 6 hrs. A quicker method is 15 min rod adhesive epoxy. Sets up within 30min. Let dry. I thin a little w/isopropyl alcohol to make it flow around the thread wrap.
BTW the hook teasers look real nice.
Posted from my iPhone/Mobile device
|
Thank you for the compliment and for the advice. I think I thought it would dry glass hard immediately.
|
No boat, back in the suds.
|
|
|
01-29-2023, 05:29 PM
|
#4
|
Registered User
Join Date: Oct 2009
Location: Mansfield, MA
Posts: 577
|
I have found with UV glue the cheap stuff is well….cheap but there is different densities. I found my
Local Napa Carrie’s a UV glue kit that for the price works great and dries rock hard. I’ll try to find the name
|
It would be raining soup, and id be be standing outside with a fork
|
|
|
01-30-2023, 07:50 AM
|
#5
|
All up in the Interweb!
Join Date: Mar 2002
Location: In the dog house.
Posts: 5,198
|
Sounds like an incomplete cure from insufficient UV light. I use Bone Dry by Solarez, no need for any other coating on the threads beforehand. When my UV light batteries start to decrease power this happens. To fix it you can either use a stronger light/new batteries, or place the tacky threads in a window sill in full sunlight to finish them off.
One item of note about UV cure glue, some people have an extreme allergic reaction to the fumes and it makes their face puff up and get all red. It's actually pretty bad for those who it bothers.
|
Co-Host of The Surfcast Podcast
"Out there in the surf is where it's at, that's where the line gets drawn in the sand between those who talk fishing and those who live it."
- a wise man.
One good fish, a sharpie does not make...
Certified rock hopping billy goat.
|
|
|
01-30-2023, 11:30 AM
|
#6
|
Very Grumpy bay man
Join Date: Nov 2003
Location: Rhode Island
Posts: 10,666
|
Thanks guys. I'm gonna buy a new light. In the mean time, I'm putting a dozen at a time in the sun.
|
No boat, back in the suds.
|
|
|
01-30-2023, 07:08 PM
|
#7
|
Afterhours Custom Plugs
Join Date: Mar 2004
Location: R.I.
Posts: 8,611
|
Solarez makes a tack free uv resin that works.
|
|
|
|
02-01-2023, 11:06 AM
|
#8
|
Very Grumpy bay man
Join Date: Nov 2003
Location: Rhode Island
Posts: 10,666
|
Quote:
Originally Posted by afterhours
Solarez makes a tack free uv resin that works.
|
Thank you sir!
|
No boat, back in the suds.
|
|
|
|
Posting Rules
|
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts
HTML code is Off
|
|
|
All times are GMT -5. The time now is 06:02 PM.
|
| |