Plug Building - Got Wood? Got Plug? |
 |
12-01-2004, 06:37 PM
|
#1
|
WTF
Join Date: May 2004
Location: wareham
Posts: 1,367
|
sand paper
what grit do you guys do your final sand with? i would like to get a bit smoother, but dont want to over do it. 
|
 diamondbanger
|
|
|
12-01-2004, 06:43 PM
|
#2
|
Registered User
Join Date: Jul 2002
Location: Maine
Posts: 4,547
|
220
|
|
|
|
12-01-2004, 06:50 PM
|
#3
|
WTF
Join Date: May 2004
Location: wareham
Posts: 1,367
|
Quote:
Originally posted by MAC
220
|
cool, thats what i picked up to try.
thanks mac 
|
 diamondbanger
|
|
|
12-01-2004, 07:32 PM
|
#4
|
Super Moderator
Join Date: Aug 2000
Location: Middleboro MA
Posts: 17,125
|
100 clothback
|
|
|
|
12-01-2004, 07:47 PM
|
#5
|
"Fishbucket"
Join Date: Feb 2004
Location: Bahston Hahbah
Posts: 6,588
|
1000grit 
|
|
|
|
12-01-2004, 07:50 PM
|
#6
|
Registered User
Join Date: Nov 2003
Location: On my boat
Posts: 9,703
|
Quote:
Originally posted by thefishingfreak
1000grit
|
Mike,
Wet or dry?
And do you use blend prep !!! 
|
LETS GO BRANDON
|
|
|
12-01-2004, 07:52 PM
|
#7
|
Canceled
Join Date: Jun 2003
Location: vt
Posts: 13,425
|
Wood 100
Primer 220
|
Frasier: Niles, I’ve just had the most marvelous idea for a website! People will post their opinions, cheeky bon mots, and insights, and others will reply in kind!
Niles: You have met “people”, haven’t you?
Lets Go Darwin
|
|
|
12-01-2004, 08:07 PM
|
#8
|
"Fishbucket"
Join Date: Feb 2004
Location: Bahston Hahbah
Posts: 6,588
|
if your gonna spray silver, or other light metalics first?
at least 400 on the primer. 600 better.
light metalics REALLY highlight the grain/sand scratches 
|
|
|
|
12-04-2004, 06:47 PM
|
#9
|
Super Moderator
Join Date: Aug 2000
Location: Middleboro MA
Posts: 17,125
|
Quote:
Originally posted by #^^^^^^^^^^^&
klingspor is the best cloth Slip
nice stuff
|
which grade of klingspor? I've been using it for years, be careful where it's made, the stuff from mexico is crap
you get what you pay for, but some suppliers pass off the cheap stuff and make more dough but don't get repeat biz.
|
|
|
|
12-04-2004, 06:58 PM
|
#10
|
Hydro Orientated Lures
Join Date: Oct 2002
Location: Brockton,Ma
Posts: 8,484
|
100 aluminum oxide
|
|
|
|
12-05-2004, 10:47 AM
|
#11
|
Salt of the Earth
Join Date: Nov 2002
Location: Suburbia, RI
Posts: 1,025
|
what makes the cloth better than regular paper
i finish with 280
|
|
|
|
12-05-2004, 10:54 AM
|
#12
|
Certified Mass-hole
Join Date: Jun 2003
Location: Jackson, NJ but born and raised in Massachusetts.
Posts: 1,223
|
I sand my primer with the 150 grit sponge then dust it with 220 grit cloth. Give it an alcohol rub down and paint.
|
|
|
|
12-05-2004, 06:51 PM
|
#13
|
Salt of the Earth
Join Date: Nov 2002
Location: Suburbia, RI
Posts: 1,025
|
thanks salty, i thought that was why, just like emery paper.
|
|
|
|
 |