Plug Building - Got Wood? Got Plug?

Reply
 
Thread Tools Rate Thread Display Modes
Old 01-30-2006, 08:12 PM   #1
steelhead
Registered User
 
Join Date: Oct 2003
Location: North shore
Posts: 1,247
Okay. With the close ups, I'm seeing what I'm lookin for....
Those Rustoleum cans or autobody cans?
steelhead is offline   Reply With Quote
Old 01-30-2006, 09:39 PM   #2
eastendlu
Registered User
iTrader: (0)
 
eastendlu's Avatar
 
Join Date: Dec 2004
Location: North Fork
Posts: 2,260
Thank FF for a most exccelent tutorial.
eastendlu is offline   Reply With Quote
Old 01-30-2006, 10:55 PM   #3
thefishingfreak
"Fishbucket"
iTrader: (1)
 
thefishingfreak's Avatar
 
Join Date: Feb 2004
Location: Bahston Hahbah
Posts: 6,588
some is laquer some is enamel some is eurethane, some is mystery paint. in my life, time is money, and you only get paid $ to do it once. do-overs suk, not saying RUSH everything as things take time to flash off but heet is a big factor.nothing works in here under 70 degrees including me. wet on wet. dry over dry, dry on topwet over dry, never dry on top of wet. red over silver, never silver over red. silver sux anyway.flouresent orange under pearl white,black over blue,grain needs black to hide. sand to 400 scuff sand with gold scuff pads if you've waited too long, nib no luv me, slip likes me,
work fast, get it done. ship it out, don't %$%$%$%$ it up. looks good, customer happy,i'm happy, paint loves me, i get paid, wife happy.
get it done, 1 hour start to finish, none of this two days to dry stuff.if it works it works if it don't it don't, try again.

thefishingfreak is offline   Reply With Quote
Old 01-30-2006, 11:02 PM   #4
fishaholic18
Finally
iTrader: (0)
 
fishaholic18's Avatar
 
Join Date: Jan 2003
Location: FL
Posts: 7,181
Quote:
Originally Posted by thefishingfreak
some is laquer some is enamel some is eurethane, some is mystery paint. in my life, time is money, and you only get paid $ to do it once. do-overs suk, not saying RUSH everything as things take time to flash off but heet is a big factor.nothing works in here under 70 degrees including me. wet on wet. dry over dry, dry on topwet over dry, never dry on top of wet. red over silver, never silver over red. silver sux anyway.flouresent orange under pearl white,black over blue,grain needs black to hide. sand to 400 scuff sand with gold scuff pads if you've waited too long, nib no luv me, slip likes me,
work fast, get it done. ship it out, don't %$%$%$%$ it up. looks good, customer happy,i'm happy, paint loves me, i get paid, wife happy.
get it done, 1 hour start to finish, none of this two days to dry stuff.if it works it works if it don't it don't, try again.
Flat Rate???

F-18®
It IsWhat It Is


¸.·´¯`·.¸><((((º>¸.·´¯`·.¸><((((º>¸.·´¯`·.¸><((((º >¸.·´¯`·.¸><((((º>¸.·´¯`·.¸><((((º>¸.·´¯`·.¸><(((( º>
fishaholic18 is offline   Reply With Quote
Old 01-30-2006, 11:06 PM   #5
thefishingfreak
"Fishbucket"
iTrader: (1)
 
thefishingfreak's Avatar
 
Join Date: Feb 2004
Location: Bahston Hahbah
Posts: 6,588
Quote:
Originally Posted by fishaholic18
Flat Rate???
plus commision

thefishingfreak is offline   Reply With Quote
Old 01-31-2006, 12:00 AM   #6
Canalman
Calling Jon The Fisherman
iTrader: (0)
 
Canalman's Avatar
 
Join Date: Jan 2003
Location: The Sack Of Mass
Posts: 2,357
Freak,

What do you use for your first coat??

-Dave

Surf Asylum Lures, Custom Lures for the "Committed"
Official S-B Sponsor
Canalman is offline   Reply With Quote
Old 01-31-2006, 12:19 AM   #7
thefishingfreak
"Fishbucket"
iTrader: (1)
 
thefishingfreak's Avatar
 
Join Date: Feb 2004
Location: Bahston Hahbah
Posts: 6,588
Dave- whear is the best place to catch a bass in febuary?
Mike


thefishingfreak is offline   Reply With Quote
Old 01-31-2006, 05:06 AM   #8
UserRemoved1
Permanently Disconnected
iTrader: (-9)
 
UserRemoved1's Avatar
 
Join Date: Nov 2002
Posts: 12,647
No he's a plug whore Dave

Quote:
Originally Posted by fishaholic18
Flat Rate???
UserRemoved1 is offline   Reply With Quote
Old 01-31-2006, 06:11 AM   #9
steelhead
Registered User
 
Join Date: Oct 2003
Location: North shore
Posts: 1,247
In the water....
steelhead is offline   Reply With Quote
Old 01-31-2006, 08:06 AM   #10
thefishingfreak
"Fishbucket"
iTrader: (1)
 
thefishingfreak's Avatar
 
Join Date: Feb 2004
Location: Bahston Hahbah
Posts: 6,588
i'll tell ya, i don't care. two part epoxy primer/sealer.
look for something that says non-sanding primer sealer and give it a try.

Last edited by thefishingfreak; 01-31-2006 at 08:14 AM..

thefishingfreak is offline   Reply With Quote
Reply

Bookmarks


Posting Rules
You may not post new threads
You may not post replies
You may not post attachments
You may not edit your posts

BB code is On
Smilies are On
[IMG] code is On
HTML code is Off

Forum Jump


All times are GMT -5. The time now is 01:11 AM.


Powered by vBulletin. Copyright ©2000 - 2008, Jelsoft Enterprises Ltd.
Please use all necessary and proper safety precautions. STAY SAFE Striper Talk Forums
Copyright 1998-20012 Striped-Bass.com